Common tensile strength grades are 1770 N/mm2, 1960 N/mm2 and 2160 N/mm2. The spinning loss factor is a pragmatical value based on the breaking load loss of the wires during the spinning process. The minimum breaking load of the rope is the product between nominal aggregate breaking load and the spinning loss factor.